| CU | ZN | SI | P | PB |
|---|---|---|---|---|
| 75.0�77.0 | Bal. | 2.7�3.4 | 0.04�0.10 | ≤0.10 |
| PROPERTY | UNIT | VALUE |
|---|---|---|
| Tensile Strength | MPa | 530�650 |
| Yield Strength (0.2%) | MPa | 260�400 |
| Elongation A50 | % | 12�25 |
| Hardness | HB | 150�200 |
| Density | g/cm� | 8.30 |
| Melting Range | �C | 880�910 |
| STANDARD | GRADE |
|---|---|
| EN | CW724R � CuZn21Si3P |
| ASTM | C69300 (EnviroBrass) � C87850 |
| DIN | 2.0375 |
| JIS | ECO Brass� |